His Excellency the Governor General in Council, on the recommendation of the Minister of Health, pursuant to section 37 of the Canada Consumer Product Safety Acta, makes the annexed Carbonated Beverage Glass Containers Regulations.S.C. 2010, c. 21InterpretationDefinition of carbonated beverage glass containerIn these Regulations, a carbonated beverage glass container means a glass container of a capacity of 1.5 L or more containing a non-alcoholic carbonated beverage.SpecificationsPerforationA carbonated beverage glass container must not, when tested in accordance with Schedule 1, shatter in such a way as to cause any piece or part of the container to perforate the plastic sheets described in that Schedule.Distance of projectionWhen a carbonated beverage glass container is tested in accordance with Schedule 2, at least 95% of the dry weight of the container must remain inside the cylinder.InformationWarningA carbonated beverage glass container must have printed on it, or affixed to it, in such a manner that the text is clearly legible, the following warning prominently displayed in boldface letters that are at least 3 mm in height:CONTENTS UNDER PRESSURE. HANDLE WITH CARE.CONTENU SOUS PRESSION. MANIPULER AVEC SOIN.Code — date of manufactureA carbonated beverage glass container must be coded in such a manner that its date of manufacture is identifiable.Quality ControlSystem of control and documentsEvery person who manufactures or imports a carbonated beverage glass container mustestablish and maintain a system of control and inspection to ensure that the carbonated beverage glass container meets the requirements set out in sections 2 and 3; andprepare and maintain documents describing tests carried out on the carbonated beverage glass container and the results of such tests.Retention period and examination by inspectorThe manufacturer or importer must keep the documents for a period of two years, and have the documents available during that period for examination by an inspector at all reasonable times.Repeal[Repeal]Coming into ForceRegistrationThese Regulations come into force on the day on which they are registered.(Section 2)Drill Test — PerforationThe following method is to be used to test whether a carbonated beverage glass container shatters in such a way as to cause perforation:as illustrated in the figure of the test apparatus, providea flat and horizontal support surface that is 10 cm in diameter,on a supporting structure of four corner posts 16 mm in diameter, four straight rods 16 mm in diameter, forming a square frame with outside dimensions of 80 cm for each side centred on the vertical centreline through the support surface and parallel to, and with the upper edges of the rods 80 cm above, the support surface,a drill probe of adjustable height, with a horizontal axial centreline in a vertical plane that passes equidistant between two opposite sides of the square frame,a sharp “MM Glazemaster Glass Drill, 4.5 mm, Type A”, affixed to and axially centred on the drill probe,a drill probe drive mechanism capable of rotating the probe 0.2 revolutions per second while advancing the drill 0.254 mm per second towards the vertical centreline through the support surface, andtwo support points for the container of adjustable height, located and oriented as shown in the figure;cover the top and the four vertical sides of the supporting structure using clear polyethylene plastic sheets of a thickness of 0.035 ± 0.005 mm, and using supplementary means of attachment as required, so thata single sheet of plastic, 80 cm wide, is suspended across the side facing the drill probe,two sheets of plastic, each 33 cm wide, are suspended on the side where the drill probe is located with a gap of 14 cm between the two sheets, symmetrical with the drill probe centreline,a single sheet of plastic, 80 cm wide, is suspended across the top and the other two sides,the lower edges of the plastic sheets extend below the plane of the support surface, andthe lower edges of the plastic sheets are subjected to a uniformly distributed downward force of 39 N/m of width by the use of weight rods;remove from the container any packaging and label that does not remain on it after its sale and during its use;ensure that the unopened container is equilibrated to a test temperature by storing it in a water bath at 22°C for four hours and is equilibrated as to pressure at that temperature by ultrasonic agitation immediately before the test;ensure that the plastic sheets are free of any perforation;adjust the drill probe and the support points to the mid-height of the container;place the container upright and unopened on the support surface and against the support points;adjust the probe drive mechanism to a linear velocity of 0.254 mm per second and a rotational velocity of 0.2 revolutions per second, and advance the drill probe until it pierces the container; andif the container shatters, note whether any piece or part of the container has perforated the plastic sheets above the horizontal plane of the support surface.The test apparatus is a square frame that is made of four corner posts connected by four straight rods. Each side of the square frame has a length of 80 cm and each corner post has a diameter of 16 mm. A carbonated beverage glass container is placed upright in the middle of the apparatus and against two support points. The two support points are situated on the side of the container opposite the drill probe and 17 mm to either side of the vertical centreline of the container. The glass drill is positioned in front of the container and perpendicular to its side. The top and each side of the test apparatus are covered in plastic sheets. The drill is moved at a fixed speed towards the container until it pierces the container.
Figure — Test Apparatus
(Section 3)Drop Test — Distance of ProjectionThe following method is to be used to test the distance of projection of a carbonated beverage glass container that has shattered:as illustrated in the figure of the test apparatus, providea block of concrete, 50 cm long, 40 cm wide and 20 cm high, having a smooth, flat and horizontal impact surface, positioned on a flat and horizontal concrete base,a rigid cylinder, with an inside diameter of 2 m and a height of 20 cm, placed vertically on the concrete base so that it is concentric with the concrete block, and the upper edge of the cylinder is in the plane of the impact surface, anda drop mechanism, consisting of two horizontal support bars of 6 mm diameter with their centrelines 4 cm apart positioned symmetrically over the longitudinal centreline of the impact surface and with their upper edges 75 cm above the impact surface, capable of permitting a free fall of the container from its horizontal support position by a snap action withdrawal of the two support bars in symmetrical paths downward and away from the container while maintaining the bar centrelines horizontal;remove from the container any packaging and label that does not remain on it after its sale and during its use;ensure that the unopened container is equilibrated to a test temperature by storing it in a water bath at 25°C for four hours and is equilibrated as to pressure at that temperature by ultrasonic agitation immediately before the test;clear and clean the area inside and outside the cylinder;place the container horizontal and unopened, centred between and on the support bars, with the vertical plane through the mid-height of the container passing through the transverse centreline of the impact surface;activate the drop mechanism allowing the container to fall freely on the impact surface;if the container shatters,collect, clean, dry and weigh all pieces and parts of the container, including the top and label, that have travelled beyond the outside diameter of the cylinder, andcollect, clean, dry and weigh all pieces and parts of the container, including the top and label, that have remained within the inside diameter of the cylinder; andcalculate the dry weight of the container by adding the weights obtained in subparagraphs (g)(i) and (ii).The test apparatus consists of a rigid cylinder, with an inside diameter of 2 m and a height of 20 cm, placed vertically on a flat and horizontal concrete base. Inside this cylinder is a block of concrete that is 50 cm long, 40 cm wide and 20 cm high. Two horizontal support bars are positioned 75 cm above the block and 4 cm apart, supporting a container that is dropped during the test.